h) Prosedur 1. Paku besi dan paku keluli dibersihkan menggunakan kertas pasir.
Procedure An iron nail and a steel nail were scrubbed with a sandpaper.
2. 5 cm3 larutan natrium klorida dituang ke dalam dua tabung uji yang berlabel A dan B.
5 cm3 of sodium chloride solution was poured into two test tubes labelled A and B.
3. Paku besi dimasukkan ke dalam tabung uji A dan paku keluli ke dalam tabung uji B.
The iron nail was put into test tube A whereas the steel nail was put into test tube B.
4. Kedua-dua tabung uji diletakkan di dalam rak tabung uji dan dibiarkan selama 4 hari.
Pemerhatian dicatatkan selepas 4 hari.
Both test tubes were placed in the test tube rack for 4 days. The observation was
recorded after 4 days.
i) Pemerhatian
Observation
Jenis paku Pengaratan paku
Type of nail Rusting of the nail
Paku besi Berkarat
PANITIA SAINS DAERAH KINTA UTARA
Iron nail Rusty
Paku keluli Tidak berkarat
Steel nail Not rusty
j) Mentafsir data Penunjuk skala :
Interpret data Scale indicator
1 Berkarat / Rusty
2 Tidak berkarat / Not rusty
3) Perbincangan a) Paku keluli lebih tahan terhadap kakisan (pengaratan).
Discussion Steel nail is more resistant to corrosion (rusting).
b) Pintu pagar besi lebih cepat berkarat berbanding dengan pintu pagar keluli.
Iron gates rust faster than steel gates.
c) Aloi adalah bahan yang tidak mengalami pengaratan dengan mudah.
An alloy is a substance which does not rust easily.