Page 229 - Template Tesis UTM v2.0
P. 229
Table E4 Summary the effect of hybridisation on the split Hopkinson pressure
bar (SHPB) properties within the strain rates of 2214 – 2350 s -1
Effect of hybridisation
Max stress (MPa)
Hybrid -1
composite (2214 – 2350) s
% Basalt % Jute % Flax %
SL (S7)
diff. (S8) diff. (S9) diff. (S10) diff.
G2/B3/G2 407.6 495.0 -17.7 524.0 -22.2
G2/J3/G2 198.9 495.0 118.0 40.7
G2/F3/G2 283.1 495.0 159.4 43.7
Table E5 Summary the effect of material selection on the split Hopkinson
-1
pressure bar (SHPB) properties within the strain rates of 700 to 2350 s
Effect of material selection
Specifc peak stress (MPa)
Hybrid
composite
700 - 850/s 1125 - 1363/s 2214 - 2350/s
G2/B3/G2 176.7 183.3 220.3
G2/J3/G2 109.2 129.6 139.1
G2/F3/G2 136.9 158.1 181.5
190