Figure 4-73: Evolution of (%) (denoted by RHF (%) in the figure) and average hydride size versus thermal cycles for a sample
with hydrogen content of 192 wppm (in Colas’ thesis this is given as 200 wppm, which is the rounded up value of 192)
cooled at 1C/min from a maximum temperature of 410C under a 230 MPa external tensile stress applied at the
maximum temperature (from [Colas et al., 2013]).