Figure 4-93:   Contour plots of the    22  stress (referred to as S22 in the figure) for, a) and c): hydride formed at 25 and 400C,
                             respectively, from a stress-free matrix and, b) and d): region of prior hydride and matrix in a) and c) after complete
                             dissolution of hydride (from [Singh et al., 2013]).