Page 157 - The Effect of Hydrogen and Hydrides - ebook first test
P. 157
Figure 4-79: Variations in relative strain derived from the changes in d-spacing of the (1 1 1) peak in a sample with 192 wppm of
δ
hydrogen heated under zero external load, then cooled under a 240 MPa external tensile stress applied in the TD
during which partial hydride reorientation occurred: (a) in the TD; and (b) in the RD (from [Colas et al., 2014]).
4.6.3.1