J, respectively while the IC sequences of [G/B]3G, [G/J]3G and [G/F]3G indicated an

                   energy value of 11.33, 18.54 and 16.80 J, respectively. It is interesting to note that the
                   ductile  of  jute  fibre  in  nature  as  reported  previously  [46]  give  an  advantage  in

                   improving  the  capacity  of  energy  absorption  than  those  of  E-glass/basalt  and  E-
                   glass/flax. In terms of peak force, the SL sequence is also exhibiting higher peak force

                   than IC sequence for all the tested hybrid composites as depicted in Figure 4.14.




                         20.0




                         18.0




                         16.0
                        Energy (J)


                         14.0




                         12.0




                         10.0
                                G 2/B 3/G 2              G 2/J 3/G 2                G 2/F 3/G 2               [G/B] 3G          [G/J] 3G           [G/F] 3G

                       Figure 4.13   Quasi-static maximum energy absorption of hybrid composites






















                                                           122