Figure 4-55:   Stress dependence for differently defined hydride reorientation ratios for irradiated BWR Zircaloy-2 cladding with liner
                             at a cooling rate of 30C/h (0.5°Cmin) (from [Aomi et al., 2009]).


                                                                                 ⁄