               Test Prod Wire




                                                  •  Stranded Tinned Copper Conductors


                                                         OD (Nom)           Insulation Thickness  Suggested Working   Breakdown
                   Part No.    AWG      Stranding                                              Voltage (VDC)  Voltage (VDC)
                                                     Inch       mm         Inch       mm

                 5000V, 90°C • Rubber Insulation
                    8899       18        65 x 36     .144       3.66       .045       1.14        5000       20,000
                 5000V, 80°C • Rubber Insulation • Manufactured for MIL-W-13169B
                    8897       18        65 x 36     .144       3.66       .045       1.14        5000       20,000
                 5000V, 80°C • PVC Insulation • UL AWM Style 1855
                    9899       18        65 x 36     .144       3.66       .048       1.22        5000        —           Hook-Up and Lead Wire
                 10,000V, 90°C • Rubber Insulation
                    8898       18        65 x 36     .229       5.82       .088       2.24       10,000      29,000
                 1000V, 90°C • Rubber Insulation • Miniature Cable
                    8890       24        45 x 40     .066       1.68       .019       .48         1000       10,000
               For available colors and put-ups, see the on-line Belden Technical Data Sheet for the part number at www.belden.com























































               PVC = Polyvinyl Chloride

                                   Fo r  m o r e  i n fo r m at i o n,  c o n t a c t   Be ld e n  Te ch n i ca l  S u ppo r t :   1- 8 0 0 - B E L D E N -1  •  www. b e l d e n . c o m
   144   145   146   147   148   149   150   151   152   153   154